Last UK despatch before Christmas: 19th December 2024. Business reopens on 3rd January 2025.

Silicone Sponge Grades: SS16,SS24,SS33

General Properties

Resistant to ultra-violet light, corona, arcing and ozone.

Excellent for vibration damping and for protecting and cushioning components.

Excellent chemical resistance (but not suitable for use with many solvents, oils or concentrated acids).

Low degree of moisture absorption, therefore the mechanical properties show little change, even after prolonged periods of immersion.

Thermal conductivity: mean average after test = 0.0695 w/(m.k.)

Not recommended for long term service where steam pressure exceeds 50 psi.

Temperature tolerance from -60° C to + 200° C.

Test Sample 10mm Thick
Grades

SS16

SS24

SS33

Apparent Density (cu.ft)

Apparent Density (cc)

16 lbs

0.25 gms

24 lbs

0.4 gms

33 gms

0.55 gms

Compression Set

15% Max

20% Max

8% Max

Compression Loading N/mm2

0.049

0.093

0.0233

Tensile Strength Mpa 3mm

1 Mpa = 145 psi 6.4mm

10 mm

1.58

1.03

0.64

1.59

1.25

0.84

2.5

2.25

1.66

Elongation @ Break 3mm

220

220

245

6.4mm 180 195 235
10mm 145 175 205

Figures given above are for guidance only and should not be used in preparation of specifications.